Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.894 g/cc | 0.0323 lb/in³ | Vibrated; ASTM D1895 |
Eastman Aqua WA314 PET
(discontinued **) Voridian Aqua PET WA314 is a polyethylene terephthalate resin designed for single-serve bottled water applications. WA314 has an intrinsic viscosity of 0.76 and provides sparkling clarity and fast i.. |
|||
Bulk Density | 0.895 g/cc | 0.0323 lb/in³ | ISO 60 |
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |