Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.975 g/cc | 0.0352 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at.. |