Polymer Property : Bulk Density = 0.0365 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.01 g/cc
0.0365 lb/in³
Loose
Excalibar ExCal® CW 100 Calcium Carbonate CaCO3 Powder
ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,..