Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.22 g/cc | 0.0441 lb/in³ | Tapped |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.22 g/cc | 0.0441 lb/in³ | Tapped |
Nyco ULTRAFIBRE® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |