Polymer Property : Bulk Density = 0.0666 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.84 g/cc
0.0666 lb/in³
Compacted
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4)
Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes ..