Polymer Property : Bulk Density = 0.0694 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.92 g/cc
0.0694 lb/in³
Packed
Excalibar ExBar™ W 4 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
Bulk Density 1.92 - 2.02 g/cc
0.0694 - 0.0730 lb/in³
Ceradyne Thermo-Sil® UHS Fused Silica
Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi..
Bulk Density 1.92 - 2.16 g/cc
0.0694 - 0.0781 lb/in³
ATI Wah Chang Reactor Grade Zirconium Oxide, ZrO2
Reactor Grade. A white, free-flowing powder.Information provided by ATI Wah ChangTypical Analysis: On Zr metal basis