Bulk Density 2.02 g/cc
0.0729 lb/in³
Dipping, 4% H2O
BNZ Materials No. 2986 Mortar
No. 2986 is a highly refractory mortar very similar to Blakbond, but gray to tan in color. Temperature to 3000°F.Information provided by BNZ Materials Inc.
Bulk Density 2.02 g/cc
0.0729 lb/in³
As received
BNZ Materials Super Blakbond Mortar
Super Blakbond is an air-setting mortar for general purpose plant use. It has greater air-setting strength than Blakbond or No. 2986. It is good for insulating fire brick where greater bond strength..