Physical Properties Metric English Comments
Bulk Density 2.33 g/cc
0.0842 lb/in³
Du-Co Ceramics S-464 Magnesia
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
Bulk Density 2.33 g/cc
0.0842 lb/in³
Chosun Refractories SF35 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.33 g/cc
0.0842 lb/in³
Chosun Refractories H-4S High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).