Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.65 - 2.75 g/cc | 0.0957 - 0.0994 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Bulk Density | 2.65 - 2.75 g/cc | 0.0957 - 0.0994 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Bulk Density | 2.65 - 2.75 g/cc | 0.0957 - 0.0994 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Bulk Density | 2.65 - 2.75 g/cc | 0.0957 - 0.0994 lb/in³ | |
Chosun Refractories CUN-738 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.65 - 2.75 g/cc | 0.0957 - 0.0994 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURON 185 T Dense Refractory Castable Description: Curon 185 T is a very pure high alumina castable based on tabular alumina with very low Fe2O3 and SiO2 contents. Suitable for use in strongly reducing atmospheres.Remarks: These values .. |