Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.85 - 2.95 g/cc | 0.103 - 0.107 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 150 G Dense Vibrating Refractory Castable Description: Vibron 150 G is a low cement castable based on sintered South-American bauxite. Especially suited for direct contact with liquid aluminum metal.Remarks: Indicated values apply to vibrat.. |
|||
Bulk Density | 2.85 - 2.95 g/cc | 0.103 - 0.107 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 150 G RAPID Dense Vibrating Refractory Castable Description: Vibron 150 G Rapid is a low cement castable based on sintered South-American bauxite. Because of special additives this material is suited for direct contact with liquid aluminum and al.. |
|||
Bulk Density | 2.85 - 2.95 g/cc | 0.103 - 0.107 lb/in³ | |
Chosun Refractories BPAP Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.85 - 2.95 g/cc | 0.103 - 0.107 lb/in³ | |
Chosun Refractories BPR-S Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.70 - 2.95 g/cc | 0.0975 - 0.107 lb/in³ | |
China-Yixing Longly Refractories Shelf Boards and Pillars SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |