Polymer Property : Bulk Density = 0.119 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 3.30 g/cc
0.119 lb/in³
MarkeTech Repton 835 Zirconia + 4 mol% Calcia
Brand 835 features: High porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal ..
Bulk Density 3.30 g/cc
0.119 lb/in³
China Tungsten YG11 Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.30 g/cc
0.119 lb/in³
China Tungsten YG12 Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.30 g/cc
0.119 lb/in³
China Tungsten YG6A Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.30 g/cc
0.119 lb/in³
China Tungsten YG9 Tungsten Carbide
Information provided by China Tungsten
Bulk Density 3.30 g/cc
0.119 lb/in³
Chosun Refractories SAL99 Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).