Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.55 - 3.65 g/cc | 0.128 - 0.132 lb/in³ | |
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
Bulk Density | 3.55 - 3.65 g/cc | 0.128 - 0.132 lb/in³ | |
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |
|||
Bulk Density | 3.55 - 3.65 g/cc | 0.128 - 0.132 lb/in³ | |
China-Yixing Longly Refractories Alumina Grinding Balls and Lining Bricks Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks Characteristics: LONGLY adopts isostatic pressing and dry pressing in the forming process. We provide a variety of products with different dimension and specification. These products are extremely.. |