Physical Properties Metric English Comments
Bulk Density 0.345 g/cc
0.0125 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons CORAX® N 375 ASTM Carbon Black
Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons.
Bulk Density 0.345 g/cc
0.0125 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons ECORAX® S 204 Carbon Black
Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons.
Bulk Density 0.345 g/cc
0.0125 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons PUREX® HS 20 Carbon Black
Carbon black grade for manufacture of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons.
Bulk Density 0.345 g/cc
0.0125 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons CORAX® N 115 ASTM Carbon Black
Standard grade of furnace black in accordance with the requirements of ASTM D 1765Hard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons.