Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® N 650 ASTM Carbon Black Standard grade of furnace black in accordance with the requirements of ASTM D 1765Soft Black - carcass grade, semi-reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | ISO 60 |
FKuR Kunststoff Fibrolon® P 8540 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 8540 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Bulk Density | >= 0.360 g/cc | >= 0.0130 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical EM600A Impact modifier for Engineering Plastics LG Chem impact modifiers for Engineering Plastics are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modifiers - Buta.. |
|||
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | ASTM D1895 |
Micropol HD Polyethylene powders for cleaning products Information provided by Micropol Limited |
|||
Bulk Density | >= 0.360 g/cc | >= 0.0130 lb/in³ | Aerated; LSY-QB-KD019 |
LG Chemical EM600 Impact modifier for Engineering Plastics Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi.. |
|||
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 S003 APS Staple Carbon Fiber, Aromatic Polymer Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 S003 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 S006 APS Staple Carbon Fiber, Aromatic Polymer Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Bulk Density | 0.360 g/cc | 0.0130 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 S006 PUT Staple Carbon Fiber, Polyurethane Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |