Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.753 g/cc | 0.0272 lb/in³ | Dry |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Bulk Density | 0.753 g/cc | 0.0272 lb/in³ | Dry |
Skamol Group Moler SUPRA Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |