Bulk Density 0.769 - 0.833 g/cc
0.0278 - 0.0301 lb/in³
Aggregate, dried, -40 mesh
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..