Physical Properties Metric English Comments
Bulk Density 0.888 g/cc
0.0321 lb/in³
Vibrated; ASTM D1895
Eastman Vitiva PC715 PET  (discontinued **)
Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi..
Bulk Density 0.888 g/cc
0.0321 lb/in³
Vibrated; ASTM D1895
Eastman CA12 PET  (discontinued **)
Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp..