Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.909 g/cc | 0.0328 lb/in³ | Vibrated; ASTM D1895 |
Eastman P76CC PET
(discontinued **) Voridian PET P76CC is used for dual ovenable containers and release paper.Applications/UsesDual ovenable containersRelease paper |