Physical Properties Metric English Comments
Bulk Density 0.920 g/cc
0.0332 lb/in³
ASTM D1895
Plenco 5350 Phenolic, Granular, Compression Molded
PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties...
Bulk Density 0.920 g/cc
0.0332 lb/in³
Asahi Glass Fluon® G350 PTFE Granular Powder
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.