Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 60 |
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Bulk Density | 0.970 - 1.03 g/cc | 0.0350 - 0.0372 lb/in³ | |
Inhance Fluoro-Seal INHANCE® Ti--9113 Titanium Carbide Polymer Alloy Product Description: INHANCE Ti-9113 polymer alloy consists of spherically shaped titanium carbide micro grains chemically bonded to surface-activated Ultra High Molecular Weight Polyethylene (UHMW.. |
|||
Bulk Density | 0.970 g/cc | 0.0350 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 200 Coating Low release at high speeds; high viscosityInformation provided by Dow Corning |
|||
Bulk Density | 0.970 g/cc | 0.0350 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 560 Coating Information provided by Dow Corning |
|||
Bulk Density | 0.970 g/cc | 0.0350 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 600 Coating Information provided by Dow Corning |
|||
Bulk Density | 0.970 g/cc | 0.0350 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 800 Coating Suitable for lamination with a variety of adhesives, maleate-inhibited coating offers improved thin film stability vs. conventional release coatings and excellent anchorage stability with super cale.. |
|||
Bulk Density | 0.970 g/cc | 0.0350 lb/in³ | |
Dow Corning SYL-OFF® PMCPSL 700 Coating Information provided by Dow Corning |