Polymer Property : Bulk Density = 1.03 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.03 g/cc
0.0372 lb/in³
ISO 60
Vyncolit W5000 Glass Fiber and Mineral Filled Novolac Phenolic
Novolac resin based, glass fiber and mineral filled. Excellent dimensional stability and very low coefficient of linear expansion and excellent chemical resistance at elevated temperatures in severa..
Bulk Density 1.03 g/cc
0.0372 lb/in³
DuPont™ Nomex® 410 Paper, 15 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..