Polymer Property : Bulk Density = 1.17 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.17 g/cc
0.0423 lb/in³
Tapped
Nyco NYGLOS® M20 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..
Bulk Density 1.17 g/cc
0.0423 lb/in³
DuPont™ Nomex® 410 Paper, 29 mil Nominal Thickness
Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is ..
Bulk Density 1.17 g/cc
0.0423 lb/in³
Tapped
Nyco ULTRAFIBRE® M20 Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..