Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novacite® 200 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novacite® Daper Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novacite® L-207A Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novacite® L-337 Untreated Lamellar Quartz Filler/Extender
Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novakup® 200 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novakup® Daper Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..
Bulk Density 1.326 g/cc
0.04789 lb/in³
Dense Packed
Malvern Minerals Novakup® L-337 Surface-Treated Lamellar Quartz Filler/Extender
Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen..