Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.39 g/cc | 0.0503 lb/in³ | In Place, dried |
St. Cloud Natural Zeolite (Clinoptilolite) Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter.. |
|||
Bulk Density | 1.39 g/cc | 0.0503 lb/in³ | Loose |
Excalibar ExBar™ 325 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Bulk Density | 1.39 g/cc | 0.0503 lb/in³ | Tapped |
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3) RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications.. |
|||
Bulk Density | 1.39 - 1.49 g/cc | 0.0502 - 0.0538 lb/in³ | |
3M #18 Roofing Granule (Corona) 3M #18 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M |