Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.08 g/cc | 0.0752 lb/in³ | Packed |
Excalibar ExBar™ 400 Barite BaSO4 Powder ExBar™ industrial barytes products are manufactured from a high-quality natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, plastics, rubber, .. |
|||
Bulk Density | 2.08 g/cc | 0.0752 lb/in³ | Packed |
Excalibar ExBar™ W 400 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |