Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.98 g/cc | 0.108 lb/in³ | |
Chosun Refractories ASC-S Alumina Silicon Carbide Carbon Bricks for Torpedo Car Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.98 g/cc | 0.108 lb/in³ | |
Chosun Refractories L12H Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.98 g/cc | 0.108 lb/in³ | |
Chosun Refractories L12HU Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.98 g/cc | 0.108 lb/in³ | |
Chosun Refractories L12S Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |