Polymer Property : Bulk Density = 4.10 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 4.10 g/cc
0.148 lb/in³
MarkeTech Repton 827 Zirconia + 3 mol% Yttria (YSZ)
Brand 827 features: Co-precipitation high porosity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, e..
Bulk Density 4.10 g/cc
0.148 lb/in³
Astro Met ZTA 96 Zirconia Toughened Alumina
General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon..