Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.075 - 0.090 µm | 0.075 - 0.090 µm | |
American Elements Gadolinium Nanoparticles General DescriptionGadolinium (Gd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Gadolinium Particles are typically 10 - 45 nanometers (nm) with sp.. |
|||
Particle Size | 0.075 - 0.090 µm | 0.075 - 0.090 µm | |
American Elements Neodymium Nanoparticles General DescriptionNeodymium (Nd) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Neodymium Particles are typically 10 - 45 nanometers (nm) with spec.. |