Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.24 µm | 0.24 µm | |
Mallard Creek Polymers Rovene® 4111 Styrene-Butadiene Emulsion Rovene® 4111 was designed with a specific particle size that greatly improves the spacing between titanium dioxide particles resulting in increased opacity. Additionally, using Rovene® 4111 ma.. |
|||
Particle Size | 0.24 µm | 0.24 µm | |
Mallard Creek Polymers Tylac® 4901 Self Stabilizing Latex Tylac® 4901 self stabilizing latex is a multi-functional styrene-butadiene copolymer additive for down hole cementing applications. Tylac® 4901 is designed for applications providing gas migra.. |