Polymer Property : Particle Size = 0.250 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.250 µm
0.250 µm
Average Stokes Equivalent Diameter
KaMin KaMin® Tek 2001 Clay
The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect..