Physical Properties Metric English Comments
Particle Size 0.39 µm
0.39 µm
Median particle diameter
Old Hickory Dunn Tennessee Ball Clay
Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an..