Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.600 µm | 0.600 µm | Average Stokes Equivalent Diameter |
KaMin KaMin® 2000C Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F.. |
|||
Particle Size | 0.600 µm | 0.600 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® 90 Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo.. |