Polymer Property : Particle Size = 0.70 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.20 - 0.70 µm
0.20 - 0.70 µm
Dispersed
Shamrock Technologies NanoFLON® P 39B Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 0.20 - 0.70 µm
0.20 - 0.70 µm
Dispersed
Shamrock Technologies NanoFLON® P 40A Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 0.20 - 0.70 µm
0.20 - 0.70 µm
Dispersed
Shamrock Technologies NanoFLON® P 51A Thermoplastic Grade PTFE Additive
Shamrock Technologies presents revolutionary new nanosized polytetraflouoroethylene (PTFE). Using this proprietary method, Shamrock can offer fully controlled distributions of PTFE in the sub-micro..
Particle Size 0.30 - 0.70 µm
0.30 - 0.70 µm
American Elements Titanium Nanoparticles
General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) ..