Polymer Property : Particle Size = 0.94 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 0.94 µm
0.94 µm
Rubber Particle Size
UBE UBEPOL BR34HL HIPS (stirring rate = 500 rpm)
Description: UBEPOL-BR34HL is characterized by its lower molecular weight and higher linear molecular chain compared with UBEPOL-BR15HB. The properties of HIPS modified by UBEPOL-BR34HL are very goo..