Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.95 µm | 1.95 µm | |
Dow FOUNDATIONS 885 High Performance Latex for Carpet Carboxylated Styrene/Acrylate Latex Applications: FOUNDATIONS 885 Latex offers properties not available in standard styrene-butadiene latexes. FOUNDATIONS 885 Latex is a high solids, low VOC acrylic latex that provides outstanding wet.. |