Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2.7 µm | 2.7 µm | Median Diameter |
Omya OMYACARB® 3 - AZ Calcium Carbonate A dry ground calcium carbonate with excellent fineness, color, and dispersion characteristics.Applications: Rubber and plastic applications such as rigid and plasticized PVC. Also used in paints, pu.. |
|||
Particle Size | 2.7 µm | 2.7 µm | Median Diameter |
Omya OMYACARB® 3 - LU Calcium Carbonate A fine, dry ground calcium carbonate with excellent color and dispersion characteristics.Applications: Rubber and plastic applications such as rigid and plasticized PVC. Also used in paints, putties.. |
|||
Particle Size | 2.7 - 8.0 µm | 2.7 - 8.0 µm | d10 |
Indium Corp. Standard ITO Indium Tin Oxide Indium Tin Oxide (ITO, or tin-doped indium oxide) is a mixture of indium(III) oxide and tin(IV) oxide, typically 90% indium oxide, 10% tin oxide by weight. In powder form it is yellow-green in colo.. |
|||
Particle Size | 2.7 µm | 2.7 µm | Rubber Particle Size |
UBE UBEPOL BR15HL HIPS (n-DM =0.03 wt %) Description: UBEPOL-BR15HL is a linear type of polymer with the high solution viscosity. In case of enlarging the dispersed rubber particle size in |
|||
Particle Size | <= 2.7 µm | <= 2.7 µm | D98 |
CIMBAR NANO-FLEX® Talc - D for TPO Applications NANO-FLEX® Talc is designed for use in high performance TPO applications that require high brightness and an high balance of stiffness and toughens. NANO-FLEX® Talc is made by a proprietary proces.. |