Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 21 µm | 21 µm | Median Diameter |
Omya SNOWHITE® 21 - PT Calcium Carbonate A dry ground calcium carbonate with a medium and closely sized particle distribution and excellent shrink resistance properties.Applications: Ideal for joint compounds, unsaturated polyester, cement.. |
|||
Particle Size | 21 - 25 µm | 21 - 25 µm | 50% |
H.C. Starck Amperit® 151.065 Tantalum (Ta) |
|||
Particle Size | 21 - 25 µm | 21 - 25 µm | 50% |
H.C. Starck Amperit® 161.065 Niobium (Nb) |
|||
Particle Size | 21 - 25 µm | 21 - 25 µm | 10% |
H.C. Starck Amperit® 558.088 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 21 - 30 µm | 21 - 30 µm | 10% |
H.C. Starck Amperit® 827.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 21 - 30 µm | 21 - 30 µm | 10% |
H.C. Starck Amperit® 832.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Particle Size | 21 µm | 21 µm | |
Silberline 4-Allâ„¢ E 3266AR The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline Aquavexâ„¢ 1752-207S Aquavexâ„¢ grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary no.. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline SilBerCote® 5245-20Y SilBerCote® Y polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. SilBerCote® Y imparts add.. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline SilBerCote® 5245-20Z SilBerCote® Z polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. Product is typically formula.. |
|||
Particle Size | 21 µm | 21 µm | Before Conversion |
Silberline Silvet® 620-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline Sparkle Silver® 5245-AR Sparkle Silver® 5245-AR is a medium, non-leafing aluminum pigment. It provides a bright, white, clean face tone with exceptionally dark flop effect. It has narrow particle size distribution. Clos.. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline Sparkle Silvex® Premier 910-20-C Aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited of use in liquid colorant applic.. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline Silvex® 620-25-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline Silvex® 620-25-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 21 µm | 21 µm | |
Silberline Sparkle Silver® 5242-AR Sparkle Silver® 5242-AR is a medium, bright, non-leafing aluminum pigment with a narrow particle size distribution. It provides exceptional brightness and is acid resistant.Applications: Automoti.. |
|||
Particle Size | 21 µm | 21 µm | Typical |
TIMCAL TIMREX® PP 25 Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Particle Size | 21 - 25 µm | 21 - 25 µm | 10% |
H.C. Starck Amperit® 551.088 Tungsten Carbide - Chromium Carbide - Nickel 70-20-7 (W-CrC-Ni) |