Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 2200 - 3150 µm | 2200 - 3150 µm | |
SYNTHOS Koplen® 2040 F Expandable Polystyrene Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO .. |
|||
Particle Size | 2200 - 3150 µm | 2200 - 3150 µm | |
SYNTHOS Koplen® 2040 FR Expandable Polystyrene Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor.. |