Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 23.1 µm | 23.1 µm | d50 |
TIMCAL TIMREX® KS75 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |