Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 27.2 µm | 27.2 µm | d90 |
TIMCAL TIMREX® F25 Primary Synthetic P/M Special-Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |