Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 33 µm | 33 µm | median; Microtrac |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 33 µm | <= 33 µm | 90% smaller than |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | <= 33 µm | <= 33 µm | 90% smaller than |
Nyco NYAD® MD325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | <= 33 µm | <= 33 µm | 90% smaller than |
Nyco NYGLOS® MSTPO Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 33 µm | 33 µm | |
Silberline SilBerCote® PC 4852X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Particle Size | 33 µm | 33 µm | Before Conversion |
Silberline Sparkle Silver® Premier ET-2025 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 33 - 41 µm | 33 - 41 µm | 50% |
H.C. Starck Amperit® 584.1 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) |