Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 36.8 µm | 36.8 µm | d50 |
TIMCAL TIMREX® KS5-75TT Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |