Polymer Property : Particle Size = 42 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 42 µm
42 µm
Average Diameter
Potters Industries Conduct-O-Fil® SC400P18 Silver-coated Copper Particles
Applications EMI shielding, conductive adhesives, conductive paints and coatings. Advantages: Most conductive combination of metals; Dendrites give excellent compression set in FIP gaskets; Flakes ..
Particle Size 42 µm
42 µm
d90
TIMCAL TIMREX® MB44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 42 µm
42 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® SFG150 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 42 µm
42 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 42 µm
42 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® SFG6 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 42 µm
42 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® SFG75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 42 µm
42 µm
at a density of 2.03 g/cc, pressure 2.5 t/cc
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..