Polymer Property : Particle Size = 46 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 46 - 66 µm
46 - 66 µm
d90, Guaranteed
TIMCAL TIMREX® T75 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Particle Size 46 µm
46 µm
Average D50; Laser Diffraction
ALM PA 860 White Nylon 11 SLS Prototyping Polymer
Unfilled White PA 11 that is formulated for easy processing across all LS platforms. Tightly controlled particle distribution creates a smooth surface finish and excellent feature detail. Parts prod..