Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 475 µm | 475 µm | |
Asahi Glass Fluon® CD076 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Particle Size | 475 µm | 475 µm | |
Asahi Glass Fluon® CD123 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |