Particle Size | 4.5 - 5.5 µm | 4.5 - 5.5 µm | D50 |
Solvay Luminostarâ„¢ Green A Phosphor Identification: Lanthanum Cerium Terbium Phosphate coprcipitateFormula: (LaxCeyTbz) PO4Main characteristics: Good homogeneity ensured by proprietary coprecipitation process, Stability and High react.. |