Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 519.088 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 526.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 527.088 Agglomerated, Sintered Tungsten Carbide-Cobalt (WC-Co) 83-17 |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 558.088 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 65 µm | 65 µm | Before Conversion |
Silberline Silvet® 460-30-E1 Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final processi.. |
|||
Particle Size | 65 µm | 65 µm | |
Silberline Silvex® 460-15-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 65 µm | 65 µm | |
Silberline Silvex® 460-15-D Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Particle Size | 65 µm | 65 µm | <3% |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Particle Size | 65 µm | 65 µm | <3% |
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles) Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin.. |
|||
Particle Size | 65 µm | 65 µm | <3% |
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree.. |
|||
Particle Size | 65 µm | 65 µm | TEC QSD |
Trelleborg AEM Eccospheres® FTD-200 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | 65 µm | 65 µm | TEC QSD |
Trelleborg AEM Eccospheres® SI-130 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Particle Size | 65 µm | 65 µm | 50th% |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 65 µm | 65 µm | 90th% |
3M S35 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 65 µm | 65 µm | 90th% |
3M S22 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 65 µm | 65 µm | Effective Top Size |
3M S60 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 65 µm | 65 µm | 90th% |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 588.088 Chromium Carbide-Nickel Chromium 75-25 (Cr3C2-NiCr) 53/20 µm |
|||
Particle Size | 65 - 75 µm | 65 - 75 µm | 90% |
H.C. Starck Amperit® 547.074 Tungsten Carbide-Nickel 88-12 (WC-Ni) |