Polymer Property : Particle Size = 72 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 72 µm
72 µm
mean value
Potters Industries Q-Cel® 5019
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Particle Size 72 - 100 µm
72 - 100 µm
Lucite International Colacryl ® PD12 Acrylic Dental Resin
Methyl Methacrylate polymers and copolymers designed for use as fast heat curing denture base resins.Colacryl denture base resins feature fast polymerisation and a wide choice of process properties...