Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 175 m²/g | 175 m²/g | Statistical thickness surface area; ASTM D 6556 |
Orion Engineered Carbons CORAX® HP 180 HP Carbon Black Specialty black designed for excellent dry grip as required for racing tiresHard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |