Physical Properties Metric English Comments
Specific Surface Area 20.9 m²/g
20.9 m²/g
Old Hickory Volunteer Tennessee Ball Clay
A versatile clay selection for casting, pressing, or plastic forming process methods. It is similar to M-23 in mineralogy with slightly more organic content. Volunteer has very good plasticity and i..